This copper powder is manufactured using an electrolytic process. The powder particles have a unique dendritic shape that offers low apparent density and high specific surface area. Consequently, the powder is widely used in a variety of fields.
| Product Categories | Metal Powders > Electrolytic Powder |
|---|---|
| Main Applications | Energy > Power generation equipment > Powder metallurgy (oil-impregnated bearings and machinery parts) Energy > Power generation equipment > Conductive materials Energy > Power generation equipment > Carbon brushes Electronics > Electronic parts (conductor materials) Automobiles > Carbon brushes Automobiles > Conductive materials Automobiles > Powder metallurgy (oil-impregnated bearings and machinery parts) Automobiles > Friction materials |
| Main ingredients | Cu (copper) |
| Manufacturing method | Electrodeposition |
| Shape | Dendritic |
| Features |
This dendritic powder features low apparent density, high specific surface area, high purity, good compactibility, good sinterability, and high conductivity. It is used extensively as a raw material in oil-impregnated bearings, sintered machinery parts, carbon brushes, and friction materials. |
| Grade | Apparent density (g/cm3) |
Flow Rate |
Particle Size Distribution (mass %) | ||||||
|---|---|---|---|---|---|---|---|---|---|
| +180 μm | +150 μm | +106 μm | +75 μm | +63 μm | +45 μm | -45 μm | |||
| CE-5A | 2.00-2.40 | ≦45 | ≦10 | Bal. | ≦15 | ≦10 | ≦15 | ||
| CE-6F |
2.10-2.30 |
≦40 | - | ≦1 | 10-25 | 30-40 | 15-25 | 10-25 | 10-20 |
| CE-8A |
1.60-1.90 |
≦50 | - | ≦3 | 5-15 | 20-35 | 10-25 | 10-30 | 15-30 |
| CE-15 |
1.35-1.60 |
- | - | - | - | ≦5 | 20-45 | 55-80 | |
| CE-25 |
1.70-2.20 |
- | - | - | - | ≦1 | 10-25 | 75-90 | |
| FCC-115 |
0.70-1.20 |
- | - | - | - | - | ≦2 | ≦10 | ≧90 |